Solubility limit of nitrogen in Fe–Cr–C–N alloy melt under reduced N2 partial pressure
Loading...
Access rights
openAccess
acceptedVersion
URL
Journal Title
Journal ISSN
Volume Title
A1 Alkuperäisartikkeli tieteellisessä aikakauslehdessä
This publication is imported from Aalto University research portal.
View publication in the Research portal (opens in new window)
View/Open full text file from the Research portal (opens in new window)
View publication in the Research portal (opens in new window)
View/Open full text file from the Research portal (opens in new window)
Unless otherwise stated, all rights belong to the author. You may download, display and print this publication for Your own personal use. Commercial use is prohibited.
Date
Major/Subject
Mcode
Degree programme
Language
en
Pages
5
Series
Vacuum, Volume 182
Abstract
The N solubility in Fe–Cr–C–N melt was measured by the addition of Cr and C in liquid iron using the metal/gas equilibration technique at 1600 °C under a reduced N 2 partial pressure. Cr increased the N solubility by the attraction force between Cr and N, while C showed the opposite effect on N in liquid iron. The present experimental results were thermodynamically analyzed by Wagner's interaction parameter formalism. The existence of the simultaneous effect of Cr and C on the N solubility was confirmed, which was determined as the second-order cross-product parameter of Cr and C on N in liquid iron. This parameter set in the multicomponent Fe–Cr–C–N system can be used to predict the solubility limit of N in the degassing process of stainless steelmaking.
Description
Other note
Citation
Paek, M-K, Lindberg, D & Pak, J-J 2020, 'Solubility limit of nitrogen in Fe–Cr–C–N alloy melt under reduced N2 partial pressure', Vacuum, vol. 182, 109726. https://doi.org/10.1016/j.vacuum.2020.109726