Upgrading copper slag cleaning tailings for re-use

dc.contributorAalto-yliopistofi
dc.contributorAalto Universityen
dc.contributor.authorHolland, Keiranen_US
dc.contributor.authorEriç, R. Hürmanen_US
dc.contributor.authorTaskinen, Pekkaen_US
dc.contributor.authorJokilaakso, Arien_US
dc.contributor.departmentDepartment of Chemical and Metallurgical Engineeringen
dc.contributor.groupauthorMetallurgical Thermodynamics and Modellingen
dc.contributor.groupauthorMetallurgy (MTG)en
dc.contributor.organizationAalto Universityen_US
dc.date.accessioned2019-03-05T10:15:20Z
dc.date.available2019-03-05T10:15:20Z
dc.date.embargoinfo:eu-repo/date/embargoEnd/2021-01-11en_US
dc.date.issued2019-03-15en_US
dc.description.abstractTailings from an industrial copper slag cleaning milling and flotation circuit have been pre-reduced at low temperatures, well below its melting point, using CH4-H2-Ar mixtures with the aim of metallizing its iron oxide component to metallic iron. The treatment carried out at 700–900 °C, with a duration of up to 90 min, indicated a complete transformation of magnetite within the first 30 min of the process. At the same time, significant fractions of its harmful impurities, antimony, arsenic, bismuth, lead and zinc, present as oxides in the slag were reduced from magnetite and the glassy inter-granular phase, and removed from the slag as flue dust in the process off-gas. The obtained fine slag powder with low impurity contents can be melted after the pre-reduction to synthetic rock or to fast cooled slag granules for further use.en
dc.description.versionPeer revieweden
dc.format.extent8
dc.format.mimetypeapplication/pdfen_US
dc.identifier.citationHolland, K, Eriç, R H, Taskinen, P & Jokilaakso, A 2019, 'Upgrading copper slag cleaning tailings for re-use', Minerals Engineering, vol. 133, pp. 35-42. https://doi.org/10.1016/j.mineng.2018.12.026en
dc.identifier.doi10.1016/j.mineng.2018.12.026en_US
dc.identifier.issn0892-6875
dc.identifier.issn1872-9444
dc.identifier.otherPURE UUID: 9dec6f4f-5792-489f-88e1-5771f31fa450en_US
dc.identifier.otherPURE ITEMURL: https://research.aalto.fi/en/publications/9dec6f4f-5792-489f-88e1-5771f31fa450en_US
dc.identifier.otherPURE LINK: http://www.scopus.com/inward/record.url?scp=85059801211&partnerID=8YFLogxK
dc.identifier.otherPURE FILEURL: https://research.aalto.fi/files/32276756/CHEM_Holland_et_al_Pre_reduction_of_copper_slag_cleaning_tailings_2019_Minerals_Engineering.pdfen_US
dc.identifier.urihttps://aaltodoc.aalto.fi/handle/123456789/37025
dc.identifier.urnURN:NBN:fi:aalto-201903052171
dc.language.isoenen
dc.publisherElsevier
dc.relation.ispartofseriesMinerals Engineeringen
dc.relation.ispartofseriesVolume 133, pp. 35-42en
dc.rightsopenAccessen
dc.subject.keywordHydrocarbonsen_US
dc.subject.keywordReduction kineticsen_US
dc.subject.keywordSlag utilizationen_US
dc.subject.keywordSmeltingen_US
dc.subject.keywordVolatilizationen_US
dc.titleUpgrading copper slag cleaning tailings for re-useen
dc.typeA1 Alkuperäisartikkeli tieteellisessä aikakauslehdessäfi
dc.type.versionacceptedVersion

Files