Measuring current density profile in a copper electrorefining cell
dc.contributor | Aalto-yliopisto | fi |
dc.contributor | Aalto University | en |
dc.contributor.advisor | Aromaa, Jari | |
dc.contributor.author | Heikkilä, Juho | |
dc.contributor.school | Kemian tekniikan korkeakoulu | fi |
dc.contributor.supervisor | Forsén, Olof | |
dc.date.accessioned | 2015-01-30T09:55:49Z | |
dc.date.available | 2015-01-30T09:55:49Z | |
dc.date.issued | 2015-01-27 | |
dc.format.extent | 52 + 12 | |
dc.identifier.uri | https://aaltodoc.aalto.fi/handle/123456789/15075 | |
dc.identifier.urn | URN:NBN:fi:aalto-201501301800 | |
dc.language.iso | en | en |
dc.location | PK | fi |
dc.programme | MTE - Materiaalitekniikan koulutusohjelma | fi |
dc.programme.major | Materiaalien prosessointi | fi |
dc.programme.mcode | MT3002 | fi |
dc.rights.accesslevel | closedAccess | |
dc.subject.keyword | copper | en |
dc.subject.keyword | electrorefining | en |
dc.subject.keyword | current density | en |
dc.subject.keyword | current distribution | en |
dc.title | Measuring current density profile in a copper electrorefining cell | en |
dc.title | Paikallisen virrantiheyden mittaaminen kuparin raffinointielektrolyysissä | fi |
dc.type | G2 Pro gradu, diplomityö | en |
dc.type.okm | G2 Pro gradu, diplomityö | |
dc.type.ontasot | Master's thesis | en |
dc.type.ontasot | Diplomityö | fi |
dc.type.publication | masterThesis | |
local.aalto.idinssi | 50551 | |
local.aalto.openaccess | no |