Influence of deposition temperature and thickness of ALD-TiO2 on planar perovskite solar cell performance
Loading...
Access rights
openAccess
CC BY
CC BY
Creative Commons license
Except where otherwised noted, this item's license is described as openAccess
publishedVersion
URL
Journal Title
Journal ISSN
Volume Title
A1 Alkuperäisartikkeli tieteellisessä aikakauslehdessä
This publication is imported from Aalto University research portal.
View publication in the Research portal (opens in new window)
View/Open full text file from the Research portal (opens in new window)
View publication in the Research portal (opens in new window)
View/Open full text file from the Research portal (opens in new window)
Unless otherwise stated, all rights belong to the author. You may download, display and print this publication for Your own personal use. Commercial use is prohibited.
Date
Department
Major/Subject
Mcode
Degree programme
Language
en
Pages
11
Series
Applied Surface Science, Volume 736, pp. 1-11
Abstract
In perovskite solar cells (PSCs), electron transport layers (ETLs) play an important role in the selection and transport of electrons. Understanding the properties of these layers in relation to device performance is essential for optimizing solar cell efficiency and enabling their integration into emerging architectures, such as flexible solar cells. Here, we deposited TiO2 at different thicknesses using atomic layer deposition (ALD), a technique well-suited for producing uniform and pinhole-free films. The crystal structure of the layers was controlled by depositing the films at three different temperatures: 150 °C, 250 °C, and 350 °C. The layers were characterized in detail to determine the morphology (by atomic force microscopy), surface composition (by X-ray photoelectron spectroscopy) and the crystal structure (by X-ray diffraction). The TiO2 layers were then incorporated as ETLs in planar perovskite solar cells to evaluate their influence on device performance. Higher deposition temperatures led to improvements in device fill factor and open-circuit voltage, leading to more efficient solar cells. Notably, the best device performance for the ALD-TiO2 layers was achieved with films deposited at 250 °C.
Description
Publisher Copyright: © 2026 The Author(s)
Other note
Citation
Qudsia, S, Weiss, A, Sirkiä, S, Wang, F, Rosqvist, E, De Los Arcos, T, Weinberger, C, Halme, J, Kemell, M & Smått, J H 2026, 'Influence of deposition temperature and thickness of ALD-TiO 2 on planar perovskite solar cell performance', Applied Surface Science, vol. 736, 166755, pp. 1-11. https://doi.org/10.1016/j.apsusc.2026.166755